The MPC Omega creep model was developed by Dr. Martin Prager over the course of many decades and is now the standard creep model used in Part 10 of API 579-1/ASME FFS-1. This article focuses on the MPC Omega creep model by describing the model, addressing problems that can arise with it, and explaining how to fix these problems.